What are causes of cracks in outside plaster of a building
and how we prevent it during constructions?
Answers were Sorted based on User's Feedback
Answer / aung
crack can repair
to avoid causing these make sure curing,
wet the bricks before placing ,
bricks absorb water form plaster motor cause these crack also
| Is This Answer Correct ? | 15 Yes | 0 No |
Answer / aditya richie
being an exothermic reaction heat is released, for reaction
to continue properly curing is extremely nesessary . cracks
occur due to lack of or inadequate curing. curing for 28
days is necessary.
| Is This Answer Correct ? | 2 Yes | 0 No |
Answer / amy
Simple, the lime are either in powder form or during
mixture, the substance are not mixed well. Second reason
may due to loss of liquid during laying or substance left
idling too long. Upon laying to surface of brick walls. In
2 to 3 months time, hairline cracks tends to appear. to
repair these cracks, for external wall, please use ready
mix ASG to make good.
| Is This Answer Correct ? | 0 Yes | 0 No |
Answer / vengalarao
Mainly cracks form if mixing ratio is not properly done. Comonly we use 1:6 for 9" and 1:5 for 4" bricks. If mix with water and sand is not proper cracs we form
To prevent if crack observed remove the plaster and attach chicken mesh and plaster upon it
| Is This Answer Correct ? | 1 Yes | 1 No |
Answer / sjtbehera
There is very little that you can do, to prevent a plaster
ceiling from cracking. If it's going to crack, there is
nothing you can do to avoid this. However, these cracks can
easily be repaired using
Fiberglas drywall tape and finishing it with drywall joint
compound.
I have probably made this repair sound easier than it is,
but there is another alternative. You could fill the crack
with a good paintable caulking. Make sure that the caulking
you use is paintable, some silicone-based caulking aren't
paintable. If the caulking can be painted over, it will
save paintable on the tube of caulking.
| Is This Answer Correct ? | 3 Yes | 4 No |
writte a c prog. to acept 5 no. from consule and then display them back on consulte in ascending order
WHAT IS THE DIFFERENCE BETWEEN FACTOR OF SAFETY AND PARTIAL SAFETY FACTOR?
1 cft have 13.5 No of Bricks, can someone help me to answer me for it's mathematically proof?
What is change order request?
What is the outturn of Ceiling plastering
why are use steel with conc. instead use of other type materials.
4 Answers College School Exams Tests, Prathima Group,
) Design a gussetted base for a column section consisting of one sc 250 with two cover plates 300 x 25 mm carrying an axial load of 2500 KN. The S.B.C. of soil is 250 KN/m2 and the permissible bearing pressure on concrete is 4000 KN.
what is the least count of staff ?
What are the tests to be conducted on cement?
I want to change job.If You have any vacancy please contact me in this mail id-parthamitra086@gmail.com.Myself partha mitra.Diploma in civil engineer with 4+ yrs. exp.Now in kolkata.If you confirm me then I will send my detail resume to you.Also send your mail id to me.My mail id is-parthamitra086@gmail.com.I will be very much thankful to you.
what is the basic fundamental of contouring?
I have certain queries, please help to solve. a) length of pile bore is 4m.excavation quantity will be area * length where area will be pi/4 * dia*dia. Is this right? b) It is a single reamed pile of 300m dia and reamed dia is 750mm. can any body help me to calculate excavated quantity of this bulb(reamed section),, concrete quantity in bulb with showing the formulas to be used?
Civil Engineering (5086)
Mechanical Engineering (4453)
Electrical Engineering (16638)
Electronics Communications (3918)
Chemical Engineering (1095)
Aeronautical Engineering (239)
Bio Engineering (96)
Metallurgy (361)
Industrial Engineering (259)
Instrumentation (3014)
Automobile Engineering (332)
Mechatronics Engineering (97)
Marine Engineering (124)
Power Plant Engineering (172)
Textile Engineering (575)
Production Engineering (25)
Satellite Systems Engineering (106)
Engineering AllOther (1379)