What kind of components are fabricated from the
superalloys, and what are their roles?
Answers were Sorted based on User's Feedback
Answer / hardik
Typical applications are in the aerospace, industrial gas
turbine and marine turbine industry, e.g. for turbine
blades for hot sections of jet engines.
Additional applications of superalloys include the
following: gas turbines (commercial and military aircraft,
power generation, and marine propulsion); space vehicles;
submarines; nuclear reactors; military electric motors;
chemical processing vessels, and heat exchanger tubing.
| Is This Answer Correct ? | 2 Yes | 0 No |
Answer / swathi
turbine disks and components are manufactured from
superalloys
| Is This Answer Correct ? | 1 Yes | 0 No |
Define what is the difference between plaster used in gold investment casting and ceramic used in the process of investment casting of automobile engine parts and turbine blades etc. When both are used in the lost-wax method?
Will aluminum alloy like 380 or 356 settle? Meaning while in “liquid form” above melting point will the heavier elements like copper, fe, silicon, zinc etc. Settle to the bottom of the liquid/molten aluminum after a period.
Explain super alloys. What makes them useful for land-based turbines?
Explain heat treatment of brass?
What is iron ferrite and what is it used for, and where is it found?
The stress concentration is caused due to ?
What is the use of piezometer
what are the causes of scaling in cast iron, after subjecting it to annealing process.
What is the melting point of brass?
Does the extrusion process for a355 and a356 alloy effect on the amount of impact energy?
what medal conducts heat best?
Define what is the different between ferrite percentage and ferrite number?
Civil Engineering (5086)
Mechanical Engineering (4453)
Electrical Engineering (16638)
Electronics Communications (3918)
Chemical Engineering (1095)
Aeronautical Engineering (239)
Bio Engineering (96)
Metallurgy (361)
Industrial Engineering (259)
Instrumentation (3014)
Automobile Engineering (332)
Mechatronics Engineering (97)
Marine Engineering (124)
Power Plant Engineering (172)
Textile Engineering (575)
Production Engineering (25)
Satellite Systems Engineering (106)
Engineering AllOther (1379)