How can I calculate the Compressive strength of cubes after 28
days of curing?Is there any formula or ration ?
Answers were Sorted based on User's Feedback
AS PER IS CODE FORMULA WAS Fck + 1.65 S
Fck - concrete grade
for M 20 ,M 25 grade s value 4
above M 25 s value was 5
Is This Answer Correct ? | 24 Yes | 5 No |
Answer / mohsin khan
force = load/area
force is the pressure which comes after testing the cube in compressive strength machine and load is the the reading which we note and area is constant i.e 22.5 cm2
Is This Answer Correct ? | 16 Yes | 2 No |
AS PER IS CODE FORMULA WAS Fck + 1.65 S
Fck - concrete grade
for M 20 ,M 25 grade s value 4
above M 25 s value was 5
Is This Answer Correct ? | 9 Yes | 2 No |
Answer / m.koti, cosmicon group, vizag
force = load/area
force is the pressure which comes after testing the cube in
compressive strength machine and load is the the reading
which we note and area is constant i.e 22.5 mm2
Is This Answer Correct ? | 5 Yes | 0 No |
Answer / swetha
COMPRESSIVE STRENGTH OF CONCRETE IS CALCULATED BY= LOAD AT FAILURE OF THE SPECIMEN/AREA OF SPECIMEN(ie 15cm*15cm=225cm)
Is This Answer Correct ? | 1 Yes | 0 No |
after 28days curing compressive strength 100% achieved that means after 28 days 100% pressure can taken .so pressure=load/area.
load means reading of testing machine.
area =(150*150*150)=22.5 mm2 constant.
Is This Answer Correct ? | 1 Yes | 1 No |
Answer / done
Seriously I can't believe it. The formulas u r giving is for therotical value of compressive strength . u can calculate that value without making any cube. But for 28 day compressive strength there is machine which applies increasing load untill cube gets failed that load per unit area is nothing but compressive strength. Nowadays we don't have to wait for 28 days as these test are done after 2-3 days on labs n they put these result n their software which will ultimately give the final compressive strength
For more info what's app on 7249474640
Is This Answer Correct ? | 0 Yes | 0 No |
how to calculate spacing rod in column
(Project Management Topic) What are the important criteria in the successful realization of the project?
what is hook's law
What is the strength of 1:6:12 mix?
i am completed my b.tech EEE in 2009,,,iam trying the job 3+ for AUTO CAD (ELECTRICAL),, what is the market for autocad electrical in hyderabad... how to handle the intervws give some suggestions ?
In an aggregate blending plant, water is sprayed before blending is performed. If the fine content in aggregate is as high as 25 %, will not the fines form into lumps / balls and distribution will not be uniform ? Further, the fines will stick onto the interior of pug mill and its content will be low. The mixed material is stockpiled for weeks / months before use. Will it not be better that blending is done in dry condition, and water will be added only during compaction at site. Please forward your comments and suggestions.
what is the safe bearing capacity of hard murum? can we consider it 50 ton?m2
in plate load test what is the thickness of plate 20mm 5mm 50mm none
22. Are you willing to attend trainings, learn new skills and develop as a professional?
material calculations for I st coatplastering 16mm CM (1:5),second coat CM(1;3)4mm thick,pcc(1:4:8),RCC M20,lime stone masonry CM(1:6)
how much cubic feet cement contain in one bag
What was asked in isro civil interview