What is the thickness of polystyrene film?
Answer Posted / viji
3.2 microns to 18.5 microns.
| Is This Answer Correct ? | 0 Yes | 1 No |
Post New Answer View All Answers
what is partion and column chromatography
how to select short coloum and long coloumn for new molecule
if instrument calibration fails then what require to do?
why we are using hexane in calibration of number of drop per mL
I have compare C2H2-air and C2H2-N2O flame AAS on determination calcium. Both use same range of std to plot calibration curve. (2-6ppm) When i measure the sample with phosphate, KCl and LaCl, C2H2-N2O flame give false positive result, around 0.5ppm. When i measure the sample with phosphste, KCl and EDTA. C2H2-N2O flame also give 0.5ppm false positive. But both above mentioned sample would not give false positive when measured by C2H2-air flame. What is the reason?
Why a1% value is used for some product ? What is the criteria for selection a1% value ?
AT WHAT CONDITIONS WILL YOU ANALYSE A SAMPLE,WHICH ARE PRESERVED AT OTHER THAN THE AMBIENT CONDITIONS?(ie COLD STORAGE SAMPLES BELOW 20* CENTIGRADE?
In GC calibration,what is the procedure to calibrate the TCD (thermal counductivity detector)suggest ?
How we can identify process related and degradation impurity in single method with short period?
How can I develope method of dissolution by HPLC OR UV
which are the diffrent batches in the pharmaceuticals?
can i use hplc detector to uplc and why?
what are risk assement in the analytical qbd?
how to develop the icp ms method? Application of icp ms?
Describe your field experience sample type collected,sample techniques,field measurements taken and equipment used?