What is the thickness of polystyrene film?

Answer Posted / shailesh

38 micron

Is This Answer Correct ?    8 Yes 0 No



Post New Answer       View All Answers


Please Help Members By Posting Answers For Below Questions

Why sometime potassium ortho phosphate mix with acetone use for sample preparation for hplc

974


Why Ethanol is Used for Standardization of GC Head space?

3710


in dissolution if one bowl got 70 percent 2nd bowl got 80 percent and 3rd bowl got 90 percent then how proceed?

318


How to calibration of the uv spectroscopy and its test?

655


if your impurity coeluting with each other in that situation how require to set specification? is it acceptable?

355






what is biorelivent dissolution media?

294


For limit test of heavy metals in BP, Method C require that the substance is ignited at a temperature not exceeding 800 °C. Why confines such the temperature?

3483


how you fix the limits of impurities?

365


Why dissolution test is not performed in all of the products

2020


how you start the solubility study?

331


What if impurity area in control sample coming more as compared to LOQ level of impurity ?

1133


how much mass should be there in volumetric flask while in preparation of sample for assay? 

2045


can we use the same detector in HPLC as well GC and what could be the differences we can find in the final chromato graph in any aspects?

1697


HI,I CLEARED BOB CLERK EXAM. MY INTERVIEW WILL BE ON 9TH OCTOBER,2010.PLEASE SEND ME INTERVIEW QUESTIONS AND ANSWERS. THANK YOU.

1725


how you start RS method development when for new product?

279