Answer Posted / snigda
With in 2.5 hrs, the mix should use otherwise the water
content which is added in composition will absorb by mortar
and mix will become tight.
Then, we have to add the water, where water content for that
mix will increase. Because of the same, Silt content will
increase where cracks develop on the structure (for finishes)
Is This Answer Correct ? | 8 Yes | 0 No |
Post New Answer View All Answers
Define What happens to Load at yielding ?
How to calculate laplength for 3 floors
At what point does a circle start losing area when being flattened?
how to calculate the crushing strength of cement concrete paver blocks 100x100x60 mm thich.
how to prepare site mix design
how many type of admixtures for water stored structure?
What is rolling stock
manhole chamber having height of 2300 mm and thickness of brickwork is 230 mm and dia of opening covering is 560 mm and bottom length vertical is 1500 mm (1:4) brick masonry and plaster 12 mm on both sides..how to estimate the no bricks used with mortar cement bags and sand for total chamber including plaster.
if i have to draw bending moment diagram of 4 way continous span then how to create it and how to find reaction?
can u plz send me ntpc placement papers(civil engineering) at mohit_verma21@yahoo.com
How much cement and sand are required for 1 square feet of plaster at a thickness of 15 mm at a ratio of 1:4?
What is the mix propotion of M10,M15,M20,M25,M30,M40,M50.M60 cement content,aggrigate,sand and water ratio.
acceptance criteria for concrete works
What is rate for brick masonry work of 1.0 m3 in cm 1:6?
What is modular elasticity?