If I want to lab 16 mm dia. bar with 20 mm dia bar with 40D
lap length which dia.should I consider for lapping
Answer Posted / sudhir patil
As per IS 456-2000 the 50 D of lesser Dia of steel is
considered for lapping.Hence for this case the 16 mm dia
bar is considered therefore the lap length is 800 mm
Is This Answer Correct ? | 59 Yes | 2 No |
Post New Answer View All Answers
How foundation is designed, Column design and beam design
I have completed building maintenance course in mcvc stream .. can I apply for the post of " sthapstya abhiyantriki sahayyak"?
Describe about the Pile test methods, which are used in Industrial & Multistory Buildings in general.
Please tell me the quantity of cement, sand, flyash, foaming agent required for 1 cubic meter of cellular lightweight concrete blocks. also , is there any admixtures required for the CLC blocks production.
Under what circumstances should pot bearings be used instead of elastomeric bearings?
why we use 19x9x9and 20x10x10 but not other
Which is the most prominent tower of world?
What do you mean by bond? What are the different types of bonds?
we have a crushing plant and our product is experiencing flakiness and elongation over limit for granite. what is the solution to this problem? how can it be avoided and what to do differently? It is not ok for batching plants
What is rate of concrete surface rendering work per sqm
5. Two long boundary walls run parallel to each other at a center to center distance of 1 meter apart. The width and height of the first wall are 0.30 m and 2.5m respectively. While those of the second are respectively 0.18m and 3.5m. Plot the distribution of vertical stress intensity due to walls on a horizontal plane, 1m below ground level. The walls have negligible depth of foundation and are made of brick masonry (y = 19.2 kN/m cu)
What is thumb rule for deep trench excavation
how much of the strength comes from post-production curing
1.what type of the rock is most suitable for wet mix macadam in construction of road? 2.what is the highest maximum dry density and optimum moisture content can be acheive by using most suitable crush rock?
What is the usage of zoom command?