Answer Posted / biswas deb narayan
It depends on the mix used if it is M10 compressive
strength in 28 days will be 100Kg/cmsq.If it is M30
compressive strength in 28 days will be 300 kg/cmsq.
| Is This Answer Correct ? | 17 Yes | 0 No |
Post New Answer View All Answers
i want texture painting pwd data
What is chemical composion test
What is the difference between EPC,DBOOT and BOOT.
what are the strength theories for yeilding and fracture materials. state the theory more suited for 1. mild steel or 2. concrete
What is min thickness,min grade of conc & age of PQC ?
what is the price of a cubic meter of concrete on international market?
How to find the cuplock pipe qty in staging for Minor bridge?
What black man invented the clothes dryer?
What are segregation and bleeding?
How is make concrete cube?
I want to know the material required per square foot in rcc roof. i.e. steel: kg/foot, cement/foot etc.
what is tension & compression of steel bending.
Would you cause a 55-gallon drum of water to weigh more by climbing in?
1) a)to prepare mortar for bricklaying how much amount of water should be added for its maximum strength and workability(to avoid cracks which results, when high quantity of water is added)?is their a formula or ratio? b) suppose we want to make 1:3 mortar,what is the best way to measure cement ,sand and water and how? c)time before which freshly prepared mortar should be used? d)proper way to mix and make mortar? e)when should curing start after laying bricks and for how long?and also how many hours per day? f)what is shear wall (please in terms of layman lol) bookish definisions are confusing.... g) and last,acc to codes what are max no. of course that should be laid in a day.
The properties of concrete HA-30 and how does it differ with M 30 (specify the important characteristics like workability,strength,mix design,slump test value)and what is the standard relating to it