why loss of strength in concrete in 7 days cube test i am
not geting mim 7 days strength that is 67 percent for M-35
and my mix design is perfect there is no doughty,and my
results are near to 7days percentage but not 67 percent.
Answer Posted / saeng
concret will get its 100% characteristic strength after 1
year only.
Is This Answer Correct ? | 2 Yes | 8 No |
Post New Answer View All Answers
why steel tanks are provided (a) for water pressure (b) for wind pressure (c) for earthquake pressure
Anyone have sample questions for bhel interview.please send me as Iam appearing for the interview on 19th sep2008. Kindly send this to my e-mail: arun_prasath_n@yahoo.co.in
What are the main reasons for conducting pull-out tests for soil nails?
What are the advantages of building a dam on the river nile?
How to calculate the cement consumption in RR Masonry in CM 1:8 for the foundation of Ground Level Reservoir
For plate load test why we are applying pressure 3 times the proposed allowable bearing pressure? Is there any supporting standards for this?
Define What materials were used to build the Golden Gate Bridge?
what is the max. and mim. height of vertical post in informatry sign board which is used in highway projects.
can i get hindi version of is codes based on civil engineering?
what is the minimum compressive strength of clay brick
How its coming concrete grade M 20 means 1:2:4. how it coming 1:2:4.
How to fix the reinforcement in footing shorter bar at bottom and longer fix at top.
how to balance aggregate during mix design of concrete???? how to calculate moisture content like C/A,F/A and how many percentage using ice instead of water for example of we are preparing ice concrete??????
Explain what is progress payment?
what are the cube & Sylinder strength of concret M20,M25,M30,M35,M40,M60 ,M75,M10 ,M15