what is the formula for lapping length

Answer Posted / ankur shrivastav

According to IRC 21:2000, clause 304.6.2----

Development/Lap Length is depends upon various factor--
like-
1. Grade of Concrete
2. Grade of Steel
3. Bonding Zone

Lap Length will be- nx Dia
Value of n is as below-

M20 M25 M30 M35 M40 and above
Fe500 66 56 48 42 42

Fe415 55 46 40 35 35

Fe 240 65 60 55 50 50

These values belongs only for bonding zone-1*.

For Bonding zone 2- n=1.4 x value of "n" in bonding zone 1

* Bonding Zone 2- Bonding Zone 2 is a zone where bar has been bent less than 45 degree angle and more than 300 mm fresh concrete is casted below the bars.

All other locations are bonding zone 1

Is This Answer Correct ?    4 Yes 1 No



Post New Answer       View All Answers


Please Help Members By Posting Answers For Below Questions

Pls help me to arrive the rates for centering shuttering for highbay using H-frames?

1880


Minimum concrete cover in slabs, columns, beams, foundation and other st?

665


How to Rectify deep crack formed on Brick Wall? Explain the method of rectify the defect?

6347


For fine aggregate which is most suitable River sand or crusher sand & why ?

1318


What is braced excavation all about?

708






What is hybrid foundation?

679


who to find building iron rod strenth

1571


Detection of a beam & a girder are––––

1773


Define What is aggregate?

693


What is the difference between EPC,DBOOT and BOOT.

23329


What is the substitute of Mastic Asphalt?

6942


Please tell me any one, how many quantity concrete paver block fixing perday ( 8hours) per mason??

1165


What is the snap size in civil and how can we create it?

2304


The building has 12 columns of 12x9 in 3 rows of 4 each in a plot of 50'x30', The central row is strengthened with 16mm twisted rods. The roof area is 1500 sft including balconies. calculate the load factor per sft. Also indicate the number of roofs the building can withstand.

2299


how much percent are used 20mm,10mm?

1435