how lap length is increased with increase of Grade of steel?
Answer Posted / bilal ali khan
development length mostly used when beam bar are passing through column and are simply shown as ld+10d
for fe500 ld is
m40-36d
m35-40d
m30-46d
m25-49d
m20-57d
for fe415 ld is
m40-30d
m35-30d
m30-38d
m25-41d
m20-47d
| Is This Answer Correct ? | 18 Yes | 3 No |
Post New Answer View All Answers
strength vs shape factor
how to caluclate sienerge qty in construction in ap
how to tie 10 legged stirrups
Hollow block masonry in cement mortar 1:4, 40×20×20cms in superstructure take 10sqm.I want calculation of brick sand
in a corner footing of a building, column lies in one corner. in this condition i want to know if the reactive pressure of soil will be uniformly distributed throughout the footing or will be uniformly varying as in the case of eccentrical loading.
How to design staircase.plz tell me formula for the design the staircase.
Why the finite element method is lower bound solution?
what is the proper procedure in conducting a california bearing ratio penetration test on soil on cbr machine?
Sometimes the side of concrete bridges is observed to turn black in color. What is the reason for this phenomenon?
the volume of cement req for 70cum of brickwork in 1:6 cement mortar is approx is equal to 3cum 5cum 7cum 1ocum
How much cement,sand,bricks and water needed for 1square metre brick work?
How much 1 cum of M15, M20 & M25 concrete weigh?
how to determine the correctness of proportion used in cement mortor and various IS codes to determine the same?
how much cement and sand required for 1cum rr masonry
What is the different type of slump test indications?