How to rectify thermal cracks (2mm wide, 9mm deep aprx. )
developed in tremix finished concrete floor?

Answer Posted / dnyanesh marne

By using GP2 rectify the thermal cracks.

Is This Answer Correct ?    1 Yes 1 No



Post New Answer       View All Answers


Please Help Members By Posting Answers For Below Questions

can i get hindi version of is codes based on civil engineering?

3877


What are segregation and bleeding?

691


roll of DLC in road constructions

1411


how statics is different from dynamics

1242


Difference between pre-tensioning and post-tensioning.

682






hi, i am appearing in HPCL(CIVIL ENGG.)exam. plz send me placement paper of this exam if u are having

2035


2. In a container filled with each of the following materials, at a porosity of 40%, determine the upward gradient required to cause the quick condition (a) Lead shot with a G = 13.75; (b) Fibre beads with G = 2.15; (c) Sand with a G = 2.32

1891


What is the wall thickness of NP-3&NP-4 hume pipe as per I.S code

1615


What is the use of extend command?

719


WHAT GOAL DO YOU HAVE IN YOUR CARRIER?

1875


Sir, Iam Applied in rrb for the posts of Junior Engineer.I want to know about the or question previews to study well.Pl send it to shukla_varun1985@yahoo.com.

1716


what is smart building materials?

1588


How can calculate the requirement of steel bars of rcc slab for 1100 sq ft?

1486


Pls help me to arrive the rates for centering shuttering for highbay using H-frames?

1888


A super elevation of 60 cm has been provided on a 8m wide road and a curve of 260m radius .calculate the max.speed in km/hr of the vehicle that can be negotiated safely? Plz answer with full solution.thanx

1350