Answer Posted / lahbib@allinterview.com
c: 3 % max
si 1.5-1.6 after inoculation
Mn 0.7-0.9
cr 0.3
Ni 0.5
S < 0.02
P <0.04
| Is This Answer Correct ? | 1 Yes | 0 No |
Post New Answer View All Answers
What is the minimum temperature for stress relieving of astm a 519 gr.4130 material and please tell us where we can find the location.
When using mercury to recover very, fine gold from ore, what is the best way to separate the gold laden mercury from the ore?
Does the extrusion process for a355 and a356 alloy effect on the amount of impact energy?
For what reason would an aluminum casting, when applied with a powder coated paint finish, cause a poor finish to the paintwork.
Define what are the properties and application of manganese steel?
How much gold concentration should be in the organic phase (dbc) before reduction by oxalic acid solution?
What is spcc material?
Differentiate between stainless steel and alloy steel?
Why is chromium molybdenum steels used to build pressure vessels?
Why post-heating is done in alloy steel welding?
What is the function of washer?
What does allotropic mean?
How do you express pitch of gears?
what is widman statten structure?
Define what are metallurgical microscopes?