Answer Posted / divyesh s mistry(pawan group)
1) REDUCE CEMENT CONSUMPTION WHICH DECREASE THE COST OF R.C.C.
2) SELF CURED MATERIAL SO LESS CURING REQUIRED.
3) GOOD FINISH SURFACE CAN ACHIEVE.
4) COMPRESSIVE STRENGTH SHOULD BE LOWER COMPARE TO DIRECT
CEMENT USAGE INITIALLY BUT CAN ACHIEVE REQUIRED STRENGTH IN
28-DAYS.
5) REDUCES THE HEAT OF HYDRATION SO THAT THE CRACKS CANNOT
DEVELOP.
| Is This Answer Correct ? | 12 Yes | 0 No |
Post New Answer View All Answers
pls tell me , what is the water content
What is difference between engineering stress and true stress?
natucher of concrete &type of concrete?
do we decide reinforcement steel , based on bending moment ? give example with continous slab?
can i make bricks using M10 grade concrete ? and what would be the cost of a brick if we use m10 grade concrete sand and aggregates ??
1) a)to prepare mortar for bricklaying how much amount of water should be added for its maximum strength and workability(to avoid cracks which results, when high quantity of water is added)?is their a formula or ratio? b) suppose we want to make 1:3 mortar,what is the best way to measure cement ,sand and water and how? c)time before which freshly prepared mortar should be used? d)proper way to mix and make mortar? e)when should curing start after laying bricks and for how long?and also how many hours per day? f)what is shear wall (please in terms of layman lol) bookish definisions are confusing.... g) and last,acc to codes what are max no. of course that should be laid in a day.
What happens when water mixed with cowdung is used for priming instead of water for lifting water in pumps?
what is the price of a cubic meter of concrete on international market?
Mention what are the composition of a landfill?
How do we test on design and style in a software?
Define What is an ice dam sock?
How good are the Weinerberger Porotherm bricks that are being used in construction in Chennai, India. Its being used in non load bearing walls and has a compressive strength greater that 35 kg/cm^2 and a density of approx.694 - 783 kg/m3.
What is the strongest bridge for a school contest?
What is factor not to be taken in consideration in mix design?
i have to give lap joint fo 1Mtr steel of dia12mm,whenever i did mistake i cut less 5cm plz tell me how much i will give lap joint so that length comes 1Mtr