1. if only 1 slab of a floor get sagged, how could be it
repaired?
2. if any footing gives the cube result, after 28 days less
than 16 n/mm2 in spite of 20 n/mm2 what are the remedies ?
Answer Posted / venu gopal
2 reasons for saging.1) bad staging/supports. 2) bad
design. any hw if it sagged it does noteffect the next slab
casting we can cast the next one. as far as repairing of
1st slab is consern we should have a graphical
representation of sag and find out the lowest level and
highest level plot them and with the help of this date we
can fix the floor level ilttle elevated than planned and
the sagged area should be concreted (screed concret) with
good mix as per site condition.
2.if it is a big footing we cannot remove and redo. so
remove the top 200mm concret by chiping and use proper
bonding agents and introduce few more rebars through the
coloun and anchor them to the old footing and change the
shape of the footing to a triangular shape with rebars and
re concrete the top surface and additional care to be taken
at the time of casting plinth beam it is better to redesign
the plinth beam to take more load which the coloum will
carry. Note. check the mix design and use skilled manpower
while casting cubes at site. also place them in water
immediately after removing from moulds (delay in this
activity will also cause cube failure)
| Is This Answer Correct ? | 6 Yes | 0 No |
Post New Answer View All Answers
cement, sand, aggregate,reinforcement & concrete consumption per square feet in multi storeyed building
how do you stabilize a waterlogged area in road construction
Which is the direction for positive angle?
What is the sugested procedure of water purification for public supply?
How much cement and water required for cement selery????
Explain what is Hybrid Foundation?
How to Know that veriation acceptable in CPWD Work Of 1:6 Cement Mortor Received Lab test report.
Define What is diversion tunnel in a dam?
There are two buildings one taller and one shorter whose time period will be grater and similarly the frequency ?
WHAT IS THE CAUSES OF RUTTING ON FLEXIBLE PAVEMENT?
I have a slab of 20cm thickness of 20m by 4m in wich we are installing 15 tons electric panels , and we have put 4 H-shaped columns under the slab but we have done many cores in the slab which seems very normal , can you help me by telling me how to calculate the bearing capacity of the slab or give me an idea if i should increase more columns Note: load distribution area 12*1.5 m2
Concrete cover for slab, column, beam and footing?
what is the procedure involved in preparing mix design of m15 grade as per IS-10262-1982
What is the strength of 1:6:12 mix?
As per Kandal suggestions, we have implemented rolling starts on 140 (+/- 5) degrees and we kept 3 rollars to complete the rolling before falling 125 degrees and the Aggregate AIV is below 22. But When the DBM bed is being rolled 3rd high viabration, (Before 1 plain & low ,2 high Viabrations), the aggregate is getting sharp edge agg. projections are damaged. As the literature is said that, the VG-30 Grade having better control the temp. susceptibility than Penetration grade. if so we could not get this problem at site. But we are facing on site. let me know.