Golgappa.net | Golgappa.org | BagIndia.net | BodyIndia.Com | CabIndia.net | CarsBikes.net | CarsBikes.org | CashIndia.net | ConsumerIndia.net | CookingIndia.net | DataIndia.net | DealIndia.net | EmailIndia.net | FirstTablet.com | FirstTourist.com | ForsaleIndia.net | IndiaBody.Com | IndiaCab.net | IndiaCash.net | IndiaModel.net | KidForum.net | OfficeIndia.net | PaysIndia.com | RestaurantIndia.net | RestaurantsIndia.net | SaleForum.net | SellForum.net | SoldIndia.com | StarIndia.net | TomatoCab.com | TomatoCabs.com | TownIndia.com
Interested to Buy Any Domain ? << Click Here >> for more details...

what are the ores of copper?

Answer Posted / guest

sulphide ore:
chalcopyrite
chalcocite
bornite
oxide ore
malachite
azurite
cuprite

Is This Answer Correct ?    1 Yes 0 No



Post New Answer       View All Answers


Please Help Members By Posting Answers For Below Questions

Explain heat treatment of brass?

926


What is the atomic density of ceramics?

1001


In welding, arc is too long due to ?

1006


How can you find out what kind of stainless steel was used in making a stainless object?

979


Why is it so hard to find literature on the wear resistance of titanium?

1294


Which of different types of cast irons is stronger? Is their strength superior to steels?

844


what are the causes of scaling in cast iron, after subjecting it to annealing process.

2369


Differentiate between 304 and 316 grades of steel?

864


How to calculate heat affected zone in weld?

1061


Which type of key is used between shaft and pulley?

897


The stress concentration is caused due to ?

1144


Is it possible to use metallurgical inverted microscope to other designation?

949


what is the chemical composition of ceramic and define what is its atomic density?

947


Why post-heating is done in alloy steel welding?

984


The requirement for ASTM A217 Gr. WC9 castings for valves components like Body and Bonnet were Normalising at 920+/- 20 Deg. C and Tempring 780+/- 20 Deg. C The specification calls furnace shall be calibtated within +/-14 deg. C The Heat Chart shows minimum temperature for normalising 900 to 920 Deg. C, but maximum temperature 960-990 Deg. C Tempering 780+/-20 Deg. C is within limits and accepted. Casting having integral test bars, heat trated along with castings passed in chemical znalysis and mechanical properties. Since normalising maximum temperature is not meeting specification, where castings can be salvaged or renormalised and retempered to meet specification. Whether it will have affect on remechanical properties testing

2190